Key Characteristics:- High gloss and clarity
- Contains 3200 ppm slip agent and 2400 ppm antiblocking agent
Recommended Applications: - Water-quench blown film for general purpose bags such as vegetable or fruit packaging
Information provided by SCG Chemicals |