MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Flexible B7D00 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 787815 sec; ASTM D2240
Tensile Strength at Break 29.7 MPa4310 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 180 %180 %Type IV, 510 mm/min; ASTM D638
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 - 196 °C365 - 385 °F
 193 - 204 °C379 - 399 °F
 
Descriptive Properties
FeaturesMedium Gloss
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFencing & Decking
 General Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex APEX® RE 8114 UV Polyvinyl Chloride, Rigid
Overview of materials for PVC, Extruded
Geon® Performance Solutions Vinyl Wire & Cable W9200 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable 3311-xx23D Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Rigid Extrusion LR840 Polyvinyl Chloride, Rigid

PH0POL1000 / 145569

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.