MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ThyssenKrupp SECURE 200 Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to heavy plates from 3 to 15 mm in thickness made of the high-strength armour steel SECURE 200 (ThyssenKrupp armour steel) with a minimum hardness of 200 HBW and a minimum tensile strength of 690 MPa for civil use.

Application: The steels may be used for the manufacturing of devices suitable for the saving of valuables, e.g. automatic tellers and safes.

Properties are typical of 12.5 mm plate thickness.

Information Provided by Thyssen Krupp

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 550 MPa79800 psi
Elongation at Break 15 %15 %
Charpy Impact 30.0 J
@Temperature -40.0 °C
22.1 ft-lb
@Temperature -40.0 °F
Longitudinal
Bend Radius, Minimum 2.0 t2.0 t2x the test piece thickness
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.14 %<= 0.14 %
Iron, Fe >= 96.3 %>= 96.3 %As Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.30 %<= 0.30 %
Niobium, Nb (Columbium, Cb) <= 0.10 %<= 0.10 %
Other <= 0.42 %<= 0.42 %Carbon Equivalent
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si <= 0.60 %<= 0.60 %
Sulfur, S <= 0.010 %<= 0.010 %
Vanadium, V <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ceradyne Ceralloy® 546-4E Boron Carbide
ExxonMobil Exxsol™ D30 Dearomatized Fluid
Momentive Performance Materials AC6043 Titanium Diboride/Boron Nitride Composite
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder
H.C. Starck Grade HP Boron Carbide, B4C

NTHYSS039 / 90359

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.