MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Duratron™ T4501 PAI Polyamide-imide, compression molded bearing grade
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Molded

Material Notes: Available in larger dimensions, this grade offers excellent compressive strength and wear behavior even in harsh thermal, chemical, and stress conditions.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Water Absorption at Saturation 1.50 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 70.0ASTM D785
Hardness, Shore D 86.0ISO 868
Tensile Strength 110 MPaISO 527-1/-2 (7)
Flexural Strength 155 MPaISO 178 (12)
Compressive Yield Strength 39.0 MPa
@Strain 1.00 %
ISO 604 (10)
 72.0 MPa
@Strain 2.00 %
ISO 604 (10)
 130 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 4.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 6.00
@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.0420
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µin/in-°FASTM E-831 (TMA)
 35.0 µm/m-°C
@Temperature 23.0 - 100 °C
 35.0 µm/m-°C
@Temperature 23.0 - 150 °C
 40.0 µm/m-°C
@Temperature >=150 °C
Thermal Conductivity 0.540 W/m-K
 3.70 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 534 °FASTM D648
Minimum Service Temperature, Air -50.0 °C
Glass Transition Temp, Tg 527 °FDMA- Tan d
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Acceptable
Continuous Sunlight Acceptable
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Duratron™ T4503 PAI Compression Molded, Polyamide-imide, Electrical Grade
Mitsubishi Chemical Advanced Materials Duratron™ T5530 PAI Compression Molded Glass Reinforced Polyamide-imide
Mitsubishi Chemical Advanced Materials Duratron™ T4301 PAI Polyamide-imide, extruded bearing grade
Mitsubishi Chemical Advanced Materials Duratron™ T4203 PAI Extruded Polyamide-imide
Mitsubishi Chemical Advanced Materials Duratron™ T7530 PAI Compression Molded Carbon Fiber Reinforced Polyamide-Imide

P1SM43 / 20138

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.