MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGO® Antifoam 5-27 Emulsion
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam 2-57 is an antifoam emulsion based on organo-modified siloxanes.

Application: TEGO® Antifoam 2-57 may be used for foam control in a variety of industrial applications, e. g.

  • during processing and application of polymer dispersions
  • in concrete plasticizers based on lignin sulfo-nate, naphthalene sulfonate and melamine sulfonate
  • in processing and application of pressure-sensitive adhesives
Properties / Benefits: As well as excellent foam control TEGO® Antifoam 2-57 provides additional benefits including:
  • excellent compatibility as pre-defoamer in various polymer dispersion applications (including PSA)
  • no negative effects in downstream applications (no surface defects, fish eyes etc.)
  • easy incorporation into concrete plasticizers and excellent storage stability (no separation)
  • improvement of concrete flowability
  • good compatibility with rubber hoses/ gaskets

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccDIN 51757
pH <= 8.0
 
Descriptive Properties
Appearancewhite emulsion
Content20%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Autoclaved aerated concrete, 0.800 g/cc density
Cymat A35620SC 020SS Stabilized Aluminum Foam
Autoclaved aerated concrete, 0.830 g/cc density
Autoclaved aerated concrete, 0.750 g/cc density
Autoclaved aerated concrete, 0.700 g/cc density

PEVONIL536 / 196740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.