MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Amadol CMA 5
Categories: Other Engineering Material

Material Notes: Ethoxylated cocoamide mainly used as wetting and dispersing agent in several applications

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
pH 6.0 - 8.06.0 - 8.01% in water
Viscosity 150 cP150 cP
Surface Tension 30 dynes/cm30 dynes/cmaccording to Du Noüy, 25°C, 0.1%; DIN 53914
 
Thermal PropertiesMetricEnglishComments
Pour Point 7.00 °C44.6 °F
Flash Point >= 100 °C>= 212 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 19 - 21 %19 - 21 %
 
Descriptive Properties
AppearanceClear red-yellow liquid
Clear point18°C
Cloud point80°C5 g product in 25 ml 25% butyldiglycol
Content(%)80Active content
HLB11.1Griffin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY117 / 285640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.