MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper, UNS C51100, H08 Temper strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability.

Applications: bridge bearing plates, locator bars, fuse clips, sleeve bushings, springs, switch parts, truss wire, wire brushes, chemical hardware, perforated sheets, textile machinery, welding rod.

Test specimen: strip - 1mm thickness.

Key Words: PB101, ISO CuSn4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9393
Hardness, Rockwell 30T 7979
Tensile Strength, Ultimate 675 MPa97900 psi
Tensile Strength, Yield 655 MPa
@Strain 0.2 %
95000 psi
@Strain 0.2 %
Elongation at Break 3.0 %3.0 %In 50mm
Modulus of Elasticity 110 GPa16000 ksi
Poissons Ratio 0.3410.341
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 41.0 GPa5950 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000870 ohm-cm
@Temperature 20.0 °C
0.00000870 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
9.89 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 84.0 W/m-K
@Temperature 20.0 °C
583 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 975 - 1060 °C1790 - 1940 °F
Solidus 975 °C1790 °F
Liquidus 1060 °C1940 °F
Annealing Point 482 - 677 °C900 - 1250 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 475 - 675 °C887 - 1250 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 94.5 - 96.3 %94.5 - 96.3 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P 0.0030 - 0.35 %0.0030 - 0.35 %
Tin, Sn 3.5 - 4.9 %3.5 - 4.9 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphor bronze 5% Sn, UNS C51000, H08 Temper flat products
Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze
Copper, UNS C51100, OSO50 Temper strip
Copper, UNS C51100, OSO35 Temper strip
Ampco Metal AMPCOLOY® 712 Tin Bronze, Castings

MC51100c2 / 11531

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.