MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BP Amoco Fortilene® KB4176 Blow Molding/Extrusion Grade Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: An anti-stated, polypropylene, random copolymer produced by Solvay Polymers utilizing unique, catalyst technology. It is designed for blow molding and extrusion applications and exhibits good stiffness and improved cycles. Meets FDA requirements of 21CFR 177.1520. This resin is Kosher certified.

Information provided by Solvay Polymers.

This product is not listed in the standard Innovene product line. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortilene® Polypropylene product line from Solvay Polymers in November 2001.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.898 g/cc0.0324 lb/in³ASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272ASTM D2240
Tensile Strength, Ultimate 34.5 MPa5000 psi2 in/min; ASTM D638
Tensile Strength, Yield 28.3 MPa4100 psi2 in/min; ASTM D638
Elongation at Break 450 %450 %2 in/min; ASTM D638
Elongation at Yield 10 %10 %2 in/min; ASTM D638
Modulus of Elasticity 1.034 GPa150.0 ksiSecant at 1% strain; ASTM D638
Flexural Modulus, 1% Secant 1103 MPa160000 psi0.05 in/min; ASTM D790
Izod Impact, Notched 0.260 J/cm
@Temperature 23.0 °C
0.487 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched >= 13.35 J/cm
@Temperature 23.0 °C
>= 25.01 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOLMJ / 68298

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.