MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Silikony Polskie Polsil E2 Silicone Emulsion
Categories: Fluid; Lubricant; Silicone Base

Material Notes: POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. The following types of emulsion are manufactured:
-emulsion with methylsilicone fluid content of 36%: POLSIL® E-l, POLSIL® E-2,
-emulsion with methylsilicone fluid content of 60%, with an antistatic agent: POLSIL® E-3,
-emulsion with methylsilicone fluid content of 60%, with organic solvent: POLSIL® E-5, POLSIL® E-5S.

Antiadhesive agent for moulds in founding and plastic and rubber processing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 - 1.01 g/cc
@Temperature 20.0 °C
0.0358 - 0.0365 lb/in³
@Temperature 68.0 °F
pH 6.5 - 9.06.5 - 9.0
Viscosity <= 150 cP
@Temperature 25.0 °C
<= 150 cP
@Temperature 77.0 °F
Storage Temperature 5.00 - 30.0 °C41.0 - 86.0 °F
 
Descriptive Properties
Hygienic Certificate PZHHK/E70828/01/2006

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLSI027 / 84327

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.