POWERSIL® 735 LIGHT GRAY A/B is a low viscous two-component compound with excellent processing properties. Its vulcanizates are noted for high tracking and erosion resistance, their good mechanical properties especially for high tear strength as well as for their excellent dielectric behavior. Special features: |