MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaowool Fibralloy Preform
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Fibralloy Preforms are precisely shaped ceramic fiber based products manufactured to the desired specifications from discontinuous alumina-silicate (Kaowool®), high alumina (Saffil) fibers, ceramic powders, or blends of both. These fiber preforms are used to selectively reinforce lightweight alloys, usually aluminum.

Fibralloy Preforms are molded using a unique, closely controlled process which uniformly combine selected engineered fibers, particles, and binders. With the addition of hybrid preforms to the Fibralloy family, metal matrix composites can be tailored to meet the most demanding requirements at the most economical costs.

MMCs are manufactured through infiltration of the porous Fibralloy Preform with molten metal. Squeeze casting of liquid aluminum alloys is the best known of these processes although other alloys and casting technologies have been and continue to be developed. Selective reinforcement of the casting is also possible using one or more preforms in specific locations to enhance particular properties. This combination of familiar, affordable aluminum casting technology with Fibralloy Preforms creates MMCs with material characteristics tailored for difficult design challenges. Wear resistance, weight reduction, low thermal expansion, stiffness, and thermal fatigue resistances are key properties that may be improved with MMCs.

Features:

  • Full range of engineered ceramic fiber compositions
  • Hybrid compositions of ceramic fibers and particles for greater design flexibility
  • Good fiber cleaning technology which creates high quality preforms time after time
  • Small development runs up to full scale production
  • Applications:

  • Diesel piston crown
  • Piston ring groove
  • Engine cylinder liner
  • Accessory pulleys
  • Brake rotors, calipers, and drums
  • Drive shafts
  • Oil pump and crankcase housings
  • Frame components
  • Rocker arms
  • Turbo impellors
  • Connecting rods
  • Cylinder head

    Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 2.60 g/cc2.60 g/cc
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 1030 - 1380 MPa150000 - 200000 psi
    Modulus of Elasticity 82.7 - 117 GPa12000 - 17000 ksi
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 45 - 49 %45 - 49 %
    SiO2 51 - 55 %51 - 55 %
     
    Descriptive Properties
    Fiber Diameter, Micron2.5
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Magnesium, Mg; Annealed Sheet
    Mitsubishi Chemical Advanced Materials Altron™ PC Extruded, Unfilled, Polycarbonate
    Edinburg Plastics CAI606 PC/ABS
    Edinburg Plastics CAI406 PC/ABS
    ChevronTexaco HDAX® SAE 30 Low Ash Gas Engine Oil

    CTHERM172 / 2492

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.