MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese SO.F.TER Polifor® 20 BS/70 High Density Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.98 g/cc0.0715 lb/in³ASTM D1505
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm0.0050 - 0.0090 in/inASTM D955
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 15.0 MPa2180 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Flexural Modulus 3.10 GPa450 ksiASTM D790
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inASTM D256/A
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index >= 600 V>= 600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100 °C212 °F50°C/h at 50 N; ASTM D1525
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 240 °C392 - 464 °FCylinder Temperature
Mold Temperature 40.0 - 60.0 °C104 - 140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
301 Stainless Steel
Celanese SO.F.TER Polifor® 5000/V0 EPY2 Flame Retardant Polypropylene
Celanese SO.F.TER Polifor® 20 BS/25 20% Aesthetic Filled Polypropylene
Celanese SO.F.TER Polifor® 12 TR/40 40% Talc Reinforced Polypropylene
Celanese SO.F.TER Polifor® 12 TR/20 20% Talc Reinforced Polypropylene

PSOFS809 / 162273

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.