MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Polygon Composites PG-P560 Composite Cross Bar
Categories: Other Engineering Material

Material Notes: The all composite cross bar from Polygon utilizes an engineered composite structure that results in excellent retention of mechanical and physical properties at elevated temperatures. This all-composite cross bar eliminates the need for traditional metallic cross bars that are a combination of a metallic shaft encapsulated with epoxy impregnated glass fabric.

Information provided by Polygon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 175 ksiAxial
Tensile Strength, Yield 100000 psi
Modulus of Elasticity 6100 ksiAxial
Tensile Modulus 550 ksiYoung's
Compressive Strength 175000 psiAxial
Compressive Modulus 6.10e+6 psiAxial
Poissons Ratio 0.28
Shear Modulus 500 ksi
Shear Strength 7000 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 400 V/mil
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.260 BTU/lb-°F
Thermal Conductivity >= 2.00 BTU-in/hr-ft²-°F
 
Descriptive Properties
CreepNone at 12 days100°C with 14 lbs. Load–deflection
 None at 14 days65°C with 14 lbs. Load–deflection
 None at 5 days80°C with 5 lbs. Load–deflection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow AFFINITY™ SM 1350 Polyolefin Plastomer
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Hexcel® HexPly® EH04 Epoxy Resin System, M35J Fiber
Hexcel® HexPly® 954-6 Curing Cyanate Resin, K13C-2U Fiber
Hexcel® HexPly® 954-3 Curing Cyanate Resin, G80-600 Fiber

PPOLYG11 / 184510

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.