MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Röchling Polystone® PVDF DK
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Product characteristics:
  • Very good welding and processing properties
  • Especially high adhesion in the composite system and therefore especially suitable for container and plant construction
  • Especially high resistance to acids
Product applications:
  • Chemical engineering and tank building
  • Electroplating technology
  • Corrosion protection

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³DIN EN ISO 1183-1
Water Absorption <= 0.40 %<= 0.40 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7777DIN EN ISO 868
Tensile Strength, Yield 55.0 MPa7980 psiDIN EN ISO 527
Elongation at Break >= 30 %>= 30 %DIN EN ISO 527
Modulus of Elasticity 2.20 GPa319 ksiDIN EN ISO 527
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²DIN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmDIN EN 62631-3-1
Surface Resistance <= 1.00e+14 ohm<= 1.00e+14 ohmDIN EN 62631-3-2
Dielectric Constant 8.08.0IEC 60250
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 - 140 µm/m-°C55.6 - 77.8 µin/in-°FDIN 53752
Specific Heat Capacity 1.20 J/g-°C0.287 BTU/lb-°FDIN 52612
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 172 - 175 °C342 - 347 °FISO 11357-3
Maximum Service Temperature, Air 140 °C284 °Flong term
 150 °C302 °Fshort term
Vicat Softening Point 140 °C284 °FDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air 0.000 °C32.0 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9273 / 232975

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.