MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Ultra-Clean ISO Grade 32 Turbine Oil, AGMA Grade 0
Categories: Fluid; Lubricant

Material Notes: Ultra-Clean Turbine Oil is a very high quality, rust and oxidation (R&O)-inhibited circulating oil developed for use in industrial gas turbines and steam turbines, and in many other industrial applications. It provides the same performance features and long service life as Turbine Oil plus the added benefit of filtration to a typical ISO Cleanliness Code of 18/16/13, for use in circulating systems with tight tolerances where particle contamination can cause operational problems. Ultra-Clean Turbine Oil is formulated to provide excellent protection against rust, corrosion and deposit formation. It has excellent oxidation resistance and thermal stability at high temperatures to minimize sludge and varnish formation, and provide long service life. It protects system components against rust and corrosion. It has excellent water-separating properties to minimize the formation of emulsions, and is resistant to excessive foam buildup that can interfere with proper lubrication.

Applications:

  • Direct-drive gas, steam and hydroelectric turbines
  • Air tools and other pneumatic equipment lubricated through air line lubricators
  • Centrifugal and rotary air compressors
  • Lightly loaded enclosed gear drives where the OEM specifies a R&O type oil (ISO VG 68)
  • Electric motor bearings, fan bearings, and blower bearings
  • Vacuum pumps, deep-well water pumps and machine tools
Ultra-Clean Turbine Oil meets the requirements of the following industry and OEM specifications:
  • ABB G12106
  • Alstom Power HTGD 90 117, for turbines without gear drives
  • Ansaldo Energia AE94.3A &AE94.2 without gear drives (ISO VG 46)
  • ANSI/AGMA Standard 9005-E02, R&O Inhibited Oils
  • ASTM D4304-06a, Type I Turbine Oil
  • British Standard 489
  • China National Standard GB 11120-2011 L-TSA (ISO VG 32 & 68) (approved)
  • Denison Hydraulics HF-1
  • DIN 51515 Part 1, Lubricating Oils, Type L-TD
  • DIN 51517 Part 2, Lubricating Oils, Type CL
  • DIN 51524 Part 1, Hydraulic Oils, Type HL
  • General Electric GEK 46506e, GEK 32568j, GEK 27070 (obsolete), GEK 28143b (obsolete)
  • Siemens Power Generation TLV 9013 04, TLV 9013 05
  • U.S. Military MIL-PRF-17672D, Symbol 2075 T-H (ISO VG 32), 2110 T-H (ISO VG 46), 2135 T-H (ISO VG 68)
  • U.S. Steel 126
Features/Benefits:
  • Excellent oxidation resistance and thermal stability for long service life
  • Protects against sludge and varnish formation
  • Protects against rust and corrosion
  • Excellent water-separating properties
  • Low carbon-forming tendency
  • Good foam resistance
  • Meets ISO Cleanliness Code rating of 18/16/13

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.862 g/cc
Density 7.18 lb/gal
Viscosity Measurement 103Index
Saybolt Viscosity at 100°F 164 SUS
Saybolt Viscosity at 210°F 44.4 SUS
Kinematic Viscosity at 40°C (104°F) 31.8 cSt
Kinematic Viscosity at 100°C (212°F) 5.4 cSt
Oxidative Stability >= 20 hourRPVOT; ASTM D2272
 >= 15000 hourTOST; ASTM D943-04a
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.080[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -37.0 °C
Flash Point 220 °CCOC
 
Descriptive Properties
Air Release0.8 minutesASTM D3427
Copper Corrosion1aASTM D130
Demulsibility20 minutes to passASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5279 / 198532

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.