MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® NRG 1902 BK Nylon 12, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® NRG 1902 BK is a high-viscosity, plasticized and impact-modified PA 12 compound with heat and light stabilizers for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications. VESTAMID® NRG 1902 BK is characterized by easy processing and good dimensional control during pipe extrusion, especially when processing large pipe diameters. Properties of compounds based on polyamide 12 vary little with changing humidity due to low moisture absorption. Parts made of the described semi-crystalline material are characterized by exceptional impact strength, low coefficient of sliding friction and good chemical resistance. The recommended process temperature for extrusion is 220°C to 250°C. VESTAMID® NRG 1902 BK is supplied ready for use in moisture-proof bags. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Energy, Oil and Gas
Sustainability: Sustainable electricity
Delivery form: Pellets, Granules
Resistance to: Hydrolysis / hot water, UV / light / weathering, Oil / fuels
Additives: Unfilled
Applications: Tube and hose
Special Characteristics: High impact strength, Semi-crystalline, Light-stabilized, High heat resistant, High viscosity
Features: Low coefficient of friction
Color: Black
Additives: Plasticizer
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 43.0 MPaISO 527
Tensile Strength 43.0 MPaISO 527
Tensile Stress 27.0 MPa
@Strain 50.0 %
ISO 527
Elongation at Break 220 %Nominal; ISO 527
Tensile Modulus 385 MPaISO 527
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 294
Injection Velocity 200 mm/secInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption25.9 kgISO 14040, 14044
ColorBlack
Global Warming Potential2.6 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.7 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
 5.8 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7933 / 325065

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.