MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Shell Shock® Fast Brushable Urethane Plastic
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Shell Shock® FAST and Shell Shock® SLOW are thixotropic plastics that self thicken when mixed and can be brushed onto a variety of surfaces or into rubber molds. When Parts A and B are mixed in proper proportion (1A:4B by volume or 1A:5B by weight), material cures at room temperature with virtually no shrinkage to a hard, durable plastic that exhibits good compressive and flexural strength. Fully cured castings are rigid and can be sanded, primed and painted. Color effects are possible by adding SO-Strong Color Tints. Shell Shock® plastics are ideal for making fast, lightweight rigid molds for creating silicone appliances and effects (use as a replacement for ‘stone molds’). You can also brush a “gel coat” into a rubber mold and back it up with rigid foam, creating a highly detailed lightweight casting. These products can also be brushed onto styrofoam (polystyrol) as an impact resistant coating that can be sanded, primed and painted (minimum 3 coats recommended). Shell Shock® plastics can also be used to make rigid support shells for brush on rubber molds.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D-1475
Viscosity 3000 cP3000 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.00060 cm/cm0.00060 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D-2240
Tensile Strength, Ultimate 21.4 MPa3100 psiASTM D-638
Elongation at Break 0.40 %0.40 %ASTM D-638
Tensile Modulus 3.00 GPa435 ksiASTM D-638
Flexural Strength 49.3 MPa7150 psiASTM D-790
Flexural Modulus 6.76 GPa980 ksiASTM D-790
Compressive Strength 62.1 MPa9000 psiASTM D-695
Compressive Modulus 3.45 GPa500 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 57.0 °C135 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourHandling Time
Pot Life 3.00 min3.00 minASTM D-2471
 
Descriptive Properties
ColorBeige
Mix Ratio1A:4Bby volume
 1A:5Bby weight
Specific Volume17.3[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN049 / 296750

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.