MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Niche Polymer POLIXL™ PA6GI30BK PA6, 30% Fiberglass Reinforced, Impact Modified, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes:

Information provided by Niche Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D792
Moisture Absorption at Equilibrium 2.0 %2.0 %50% RH; ASTM D570
Water Absorption at Saturation 5.5 %5.5 %immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inASTM D955
Ash 30 %30 %glass-fiber; ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psiISO 527
Elongation at Break 8.0 %8.0 %ISO 527
Tensile Modulus 5.17 GPa750 ksiBreak; ISO 527
Flexural Strength 152 MPa22000 psiISO 178
Flexural Modulus 4.48 GPa650 ksiISO 178
Izod Impact, Notched (ISO) 23.0 kJ/m²10.9 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei Leona™ 54G33 Polyamide 66, GF Reinforced
Solvay APC-2-PEEK Unreinforced
Omni Plastics OmniLon™ PA6/6 U GMR40 BK1000 Nylon 6/6, 40% Glass/mineral reinforced
Niche Polymer POLISAV™ PA6GM38BK PA6, 38% Fiberglass/Mineral Reinforced
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66

PNICHE127 / 193709

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.