MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber/PTFE Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

New suppliers have been added for this product during the past 60 days.  

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.22 - 1.78 g/cc0.0441 - 0.0643 lb/in³Average value: 1.45 g/cc Grade Count:110
Filler Content 5.00 - 40.0 %5.00 - 40.0 %Average value: 23.1 % Grade Count:57
Water Absorption 0.300 - 6.00 %0.300 - 6.00 %Average value: 1.03 % Grade Count:48
Moisture Absorption at Equilibrium 0.600 - 2.00 %0.600 - 2.00 %Average value: 1.12 % Grade Count:5
Water Absorption at Saturation 0.800 - 5.50 %0.800 - 5.50 %Average value: 3.08 % Grade Count:4
Additive Loading 15.0 - 50.0 %15.0 - 50.0 %Average value: 29.6 % Grade Count:16
Linear Mold Shrinkage 0.000300 - 0.0200 cm/cm0.000300 - 0.0200 in/inAverage value: 0.00501 cm/cm Grade Count:105
Linear Mold Shrinkage, Transverse 0.00400 - 0.0140 cm/cm0.00400 - 0.0140 in/inAverage value: 0.00956 cm/cm Grade Count:12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114 - 120114 - 120Average value: 118 Grade Count:27
Tensile Strength, Ultimate 68.0 - 250 MPa9860 - 36300 psiAverage value: 138 MPa Grade Count:107
Tensile Strength, Yield 145 - 179 MPa21000 - 26000 psiAverage value: 163 MPa Grade Count:3
Elongation at Break 1.00 - 8.00 %1.00 - 8.00 %Average value: 3.26 % Grade Count:108
Modulus of Elasticity 3.00 - 13.8 GPa435 - 2000 ksiAverage value: 8.41 GPa Grade Count:100
Flexural Yield Strength 89.0 - 320 MPa12900 - 46400 psiAverage value: 209 MPa Grade Count:100
Flexural Modulus 3.03 - 20.0 GPa440 - 2900 ksiAverage value: 7.86 GPa Grade Count:98
Flexural Strain at Break 3.30 - 3.50 %3.30 - 3.50 %Average value: 3.40 % Grade Count:3
Compressive Yield Strength 68.9 - 165 MPa10000 - 23900 psiAverage value: 115 MPa Grade Count:19
Shear Strength 76.0 - 79.0 MPa11000 - 11500 psiAverage value: 77.0 MPa Grade Count:3
Izod Impact, Notched 0.427 - 2.14 J/cm0.800 - 4.01 ft-lb/inAverage value: 0.968 J/cm Grade Count:83
Izod Impact, Unnotched 3.74 - 13.3 J/cm7.00 - 25.0 ft-lb/inAverage value: 7.92 J/cm Grade Count:74
Izod Impact, Notched (ISO) 10.1 - 18.1 kJ/m²4.80 - 8.59 ft-lb/in²Average value: 13.9 kJ/m² Grade Count:5
Charpy Impact Unnotched 3.00 J/cm² - NB14.3 ft-lb/in² - NBAverage value: 5.14 J/cm² Grade Count:17
 2.70 - 4.50 J/cm²
@Temperature -40.0 - -30.0 °C
12.8 - 21.4 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 3.62 J/cm² Grade Count:5
Charpy Impact, Notched 0.350 - 1.81 J/cm²1.67 - 8.60 ft-lb/in²Average value: 0.953 J/cm² Grade Count:20
 0.300 - 1.30 J/cm²
@Temperature -40.0 - -30.0 °C
1.43 - 6.19 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 0.550 J/cm² Grade Count:3
Coefficient of Friction 0.210 - 0.3000.210 - 0.300Average value: 0.252 Grade Count:9
Coefficient of Friction, Static 0.220 - 0.3500.220 - 0.350Average value: 0.293 Grade Count:9
K (wear) Factor 5.10 - 50.4 x 10-8 mm³/N-M2.53 - 25.0 x 10-10 in³-min/ft-lb-hrAverage value: 19.9 x 10-8 mm³/N-M Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 - 1.00e+16 ohm-cm1.00e+11 - 1.00e+16 ohm-cmAverage value: 1.34e+15 ohm-cm Grade Count:62
Surface Resistance 1.00e+10 - 1.00e+15 ohm1.00e+10 - 1.00e+15 ohmAverage value: 1.40e+14 ohm Grade Count:9
Dielectric Constant 3.70 - 4.203.70 - 4.20Average value: 3.80 Grade Count:16
Dielectric Strength 18.1 - 19.7 kV/mm460 - 500 kV/inAverage value: 19.5 kV/mm Grade Count:16
Dissipation Factor 0.0130 - 0.02000.0130 - 0.0200Average value: 0.0160 Grade Count:16
Arc Resistance 100 - 120 sec100 - 120 secAverage value: 112 sec Grade Count:9
Comparative Tracking Index 550 - 600 V550 - 600 VAverage value: 567 V Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.8 - 55.8 µm/m-°C11.0 - 31.0 µin/in-°FAverage value: 38.1 µm/m-°C Grade Count:21
Thermal Conductivity 0.240 - 0.519 W/m-K1.67 - 3.60 BTU-in/hr-ft²-°FAverage value: 0.432 W/m-K Grade Count:18
Melting Point 249 - 275 °C480 - 527 °FAverage value: 258 °C Grade Count:10
Maximum Service Temperature, Air 90.0 - 180 °C194 - 356 °FAverage value: 137 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 216 - 270 °C420 - 518 °FAverage value: 249 °C Grade Count:52
Deflection Temperature at 1.8 MPa (264 psi) 190 - 260 °C374 - 500 °FAverage value: 238 °C Grade Count:98
Vicat Softening Point 200 - 252 °C392 - 486 °FAverage value: 241 °C Grade Count:17
Flammability, UL94 HB - V-0HB - V-0Grade Count:80
Glow Wire Test 700 - 960 °C1290 - 1760 °FAverage value: 872 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 310 °C500 - 590 °FAverage value: 284 °C Grade Count:34
Nozzle Temperature 280 - 300 °C536 - 572 °FAverage value: 290 °C Grade Count:4
Melt Temperature 260 - 310 °C500 - 590 °FAverage value: 289 °C Grade Count:68
Mold Temperature 60.0 - 150 °C140 - 302 °FAverage value: 88.4 °C Grade Count:100
Drying Temperature 75.0 - 120 °C167 - 248 °FAverage value: 84.5 °C Grade Count:62
Moisture Content 0.100 - 0.200 %0.100 - 0.200 %Average value: 0.191 % Grade Count:44
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:40
Injection Pressure 30.0 - 124 MPa4350 - 18000 psiAverage value: 98.7 MPa Grade Count:75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66, PTFE Filled
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite
Overview of materials for Polyamide-Imide, Glass Filled

O2518 / 78017

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.