MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Hostaform® S 27072 GV 1/10 Elastomer Modified Acetal Copolymer with 10% Glass Fiber
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 10% Glass Fiber Reinforced

Material Notes: Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials.

Specific Notes for this Grade: Easy flowing injection molding grade, elastomer-modified and reinforced with 10% w/w glass fibers. For matt and scratch-resistant surfaces.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³10x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %80x80x1mm, at 23°C and 50% RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %80x80x1mm, 23°C; ISO 62
Melt Flow 25.92 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25.92 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Calculated from Volume flow Rate: 18 cm3/10min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 110 MPa16000 psi30 sec value, 20x20x4 mm; ISO 2039, part 1; applied load 358 N
Tensile Strength, Yield 42.0 MPa6090 psimulti-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 5 mm/min
Elongation at Break 20 %20 %multi-purpose specimen (ISO 3167); ISO 527, part 1/2; test speed 5 mm/min
Elongation at Yield 8.0 %8.0 %multi-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 5 mm/min
Tensile Modulus 2.40 GPa348 ksimulti-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 1 mm/min
Flexural Modulus 2.40 GPa348 ksi80x10x4mm from multi-purpose test specimen (ISO 3167); ISO 178
Charpy Impact Unnotched 5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eU
 5.00 J/cm²
@Thickness 4.00 mm,
Temperature 23.0 °C
23.8 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eU
Charpy Impact, Notched 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eA
 0.400 J/cm²
@Thickness 4.00 mm,
Temperature 23.0 °C
1.90 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
80x80x1 mm; IEC 60250
 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
80x80x1 mm; IEC 60250
Dielectric Strength 32.0 kV/mm813 kV/in80x80x1 mm; IEC 60243, part 1
Dissipation Factor  0.0060
@Frequency 100 Hz
0.0060
@Frequency 100 Hz
80x80x1 mm; IEC 60250
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
80x80x1 mm; IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal, 30x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 11359, part 1/2
Melting Point 166 °C331 °FDSC, 10 K/min, Molding compound; ISO 3146, method C1b
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C192 °F80x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 75, part 1/2
Vicat Softening Point 135 °C275 °FVST/B/50, 10x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chase Plastics CP Pryme® AH120 Acetal Copolymer, 20% Glass Fiber Reinforced
Celanese Hostaform® S 27076 Elastomer Modified Acetal Copolymer
Celanese Hostaform® C 9021 GV1/10 POM, 10% Glass Reinforced
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM)
Celanese Celcon® GC10TF 10% Glass Fiber Reinforced, Coupled Acetal Copolymer

PHCX26 / 46056

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.