Semi-crystalline Nylon 6 (PA 6) Characteristics: Nucleated: Quick Crystallization, Excellent Flow and Release Applications: Bearings, Gears, Connectors, Automotive Housings, Power Tool Housings Processing: Injection Molding (Melt Temperature: 465-555°F, Mold Temperature: 160-195°F) Data supplied by Albis Plastics Corporation. Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off. |