MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 50% Glass Fiber Filler

Material Notes: A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.

These products have significantly improved impact performance characteristics compared to other grades of Polypropylene long fiber thermoplastics. The room temperature Charpy impact properties are 25 to 30% higher at room temperature and at low temperature (-40 C).

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM-D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 120 MPa17400 psiASTM-D638
Elongation at Break 2.1 %2.1 %ASTM-D638
Tensile Modulus 9.50 GPa1380 ksiASTM-D790
Flexural Strength 200 MPa29000 psiASTM-D790
Flexural Modulus 9.20 GPa1330 ksiASTM-D790
Izod Impact, Notched 3.50 J/cm
@Temperature 23.0 °C
6.56 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 153 °C307 °FASTM-D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled
Polyram Polytron P40B03 Copolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber
Polyram Polytron P30B03 Copolymer Polypropylene, Chemically Coupled 30% Long Glass Fiber

PPOLYRA389 / 57651

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.