MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dow Elite® 5200 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: ELITE® 5200 enhanced polyethylene resin is a copolymer produced via INSITE® Technology from Dow Plastics. This resin offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, ELITE 5200 resin provides excellent on-pallet elongation for higher yields on regular loads. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2 (a) when used unmodified and processed according to good manufacturing practices.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³
Melt Flow 4.0 g/10 min
@Load 2.16 kg
4.0 g/10 min
@Load 4.76 lb
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.3 MPa1490 psi
Film Tensile Strength at Yield, TD 8.80 MPa1280 psi
Film Elongation at Break, MD 460 %460 %
Film Elongation at Break, TD 620 %620 %
Elmendorf Tear Strength MD 320 g320 gUnspecified film thickness
Elmendorf Tear Strength TD 460 g460 gUnspecified film thickness
Dart Drop Test 300 g0.662 lb
Film Tensile Strength at Break, MD 38.6 MPa5600 psi
Film Tensile Strength at Break, TD 29.7 MPa4310 psi
 
Optical PropertiesMetricEnglishComments
Haze 0.80 %0.80 %
Gloss 95 %95 %45°
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow HDPE 10462N High Density Polyethylene
Huntsman PE5080 Extrusion Coating Polyethylene
Dow ELITE™ 5500G Enhanced Polyethylene Resin
Dow ELITE™ 5401G Enhanced Polyethylene Resin
Dow ELITE™ 5400G Enhanced Polyethylene Resin

PDW471 / 34540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.