MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ascend Performance Materials Vydyne® B 30 GF BK G/W PA6-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Vydyne B 30 GF BK G/W  is a standard flow, 30% glass-fiber reinforced PA 6 resin. This product is also lubricated to improve machine feed and flow. It is suitable for high-thickness parts.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 2.1 %2.1 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
0.0040 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.00 mm
0.0080 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psiDAM; ISO 527-2
Elongation at Break 2.5 %2.5 %DAM; ISO 527-2
Tensile Modulus 8.80 GPa1280 ksiDAM; ISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 575 V
@Thickness 3.00 mm
575 V
@Thickness 0.118 in
IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FUnannealed; DAM; ISO 75-2/A
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 255 °C446 - 491 °FInjection
Middle Barrel Temperature 235 - 260 °C455 - 500 °FInjection
Front Barrel Temperature 240 - 260 °C464 - 500 °FInjection
Nozzle Temperature 240 - 260 °C464 - 500 °FInjection
Melt Temperature 240 - 260 °C464 - 500 °FInjection
Mold Temperature 70.0 - 95.0 °C158 - 203 °FInjection
Drying Temperature 80.0 - 110 °C176 - 230 °FInjection
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection
 
Descriptive Properties
AdditiveLubricant
Agency RatingsISO, 1043 PA6 GF30
AppearanceBlack
FeaturesBalanced Stiffness/Toughness
 Bromine Free
 Chemical Resistant
 Fast Molding Cycle
 General Purpose
 Good Color Stability
 Good Impact Strength
 Good Mold Release
 Good Processability
 Good Rigidity
 Good Stiffness
 Good Strength
 Good Surface Finish
 Good Tensile Strength
 Good Toughness
 Halogen Content, None
 High Crystallinity
 High Flow
 Homopolymer
 Low Viscosity
 Lubricated
 Non-Corrosive
 Nucleated
 Thermal Stability
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8523 / 296336

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.