MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Mobility and Materials Hytrel® SC938 NC010 TPC-ET  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 30 Shore D High Performance Polyester Elastomer Developed for the Healthcare Industry

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Melt Density 0.940 g/cc
@Temperature >=177 °C
0.0340 lb/in³
@Temperature >=351 °F
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
Sim. to ISO 62
 0.80 %
@Thickness 2.00 mm
0.80 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4, 2577
Melt Flow  5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 5.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
from MVR and melt density; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3030ISO 7619-1
 26
@Time 15.0 sec
26
@Time 0.00417 hour
ISO 7619-1
Tensile Strength at Break 24.0 MPa3480 psiISO 527-1/-2
Tensile Stress at Strain  1.80 MPa
@Strain 10 %
261 psi
@Strain 10 %
ISO 527-1/-2
 5.00 MPa
@Strain 50 %
725 psi
@Strain 50 %
ISO 527-1/-2
Elongation at Break >= 300 %>= 300 %ISO 527-1/-2
 900 %900 %ISO 527-1/-2
Tensile Modulus 0.0250 GPa3.63 ksiISO 527-1/-2
Flexural Modulus 0.0250 GPa3.63 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 22.0 MPa3190 psiISO 899-1
Tear Strength 77.0 kN/m439 plinormal; ISO 34-1
 80.0 kN/m456 pliparallel; ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.9
@Frequency 100 Hz
4.9
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 177 µm/m-°C98.3 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 206 µm/m-°C114 µin/in-°FISO 11359-1/-2
Thermal Conductivity 0.150 W/m-K
@Temperature >=177 °C
1.04 BTU-in/hr-ft²-°F
@Temperature >=351 °F
Melt
Melting Point 177 °C351 °F10°C/min; ISO 11357-1/-3
Brittleness Temperature -98.0 °C-144 °FISO 974
Glass Transition Temp, Tg -60.0 °C-76.0 °F10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 205 °C374 - 401 °FExtrusion
 190 - 210 °C374 - 410 °FInjection
 200 °C392 °FExtrusion Optimum
 205 °C401 °FInjection Optimum
Mold Temperature 30.0 °C86.0 °FInjection Optimum
 30.0 - 40.0 °C86.0 - 104 °FInjection
Drying Temperature 80.0 °C176 °FExtrusion
 80.0 °C176 °FInjection
 100 °C212 °FExtrusion
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourDehumidified Dryer; Extrusion
 2.00 - 3.00 hour2.00 - 3.00 hourDehumidified Dryer; Injection
Moisture Content 0.060 %0.060 %Extrusion
 0.080 %0.080 %Injection
 
Descriptive Properties
Delivery formPellets
Drying RecommendedyesInjection
Part Marking CodeTPC-ETISO 11469
ProcessingBlow Molding
 Calandering
 Casting
 Coatable
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
Resin IdentificationTPC-ETISO 1043
Special characteristicsLight stabilized or stable to light

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Crastin® SC164 NC010 PBT
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Ineos ABS Lustran® M203FC
Lubrizol ESTANE® GP70AE Ester Based Thermoplastic Polyurethane
Celanese Hytrel® HTR8241 TPC-ET

PZDSX5230 / 197870

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.