MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 50% Cold Work
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-corrosion cracking than exhibited by the standard 300 series stainless steels, and is less costly than the traditional nickel-base corrosion resistance alloys.

The AL-6XN alloy has exhibited good performance in a variety of highly corrosive environments. The AL-6XN alloy is available in a wide range of products from including plate, strip, sheet, bar, billet, tubing pipe and castings. Its various product forms are covered by ASME and ASTM specifications. The use of wrought AL-6XN products in the ASME Boiler and Pressure Vessel is covered by Code Case 1997 (latest revision) for Section VII construction and by Code Case N-438 (latest revision) for Section III construction. This use of AL-6XN castings is covered by Code Case 2106 (latest revision) for Section VIII and Code Case 497 (latest revision) for section III construction. The alloy is approved for both welded and unwelded construction under ANSI/ASME B31.1 Code Case 155. Use of AL-6XN alloy in contact with hydrogen sulfide-containing petroleum and natural gas is covered by NACE MR0175-92.

Information provided by Allegheny Ludlum Corporation.

Key Words: AL6XN; ASTM B-688; ASME SB-688
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.06 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1280 MPa
Tensile Strength, Yield 1140 MPa
@Strain 0.2 %
Elongation at Break 3.0 %in 2" (50 mm)
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000890 ohm-cm
Magnetic Permeability 1.0028at 200 Oersted; before cold work
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.3 µm/m-°C
@Temperature 20.0 - 100 °C
 15.5 µm/m-°C
@Temperature 20.0 - 200 °C
 15.7 µm/m-°C
@Temperature 20.0 - 300 °C
 16.4 µm/m-°C
@Temperature 20.0 - 600 °C
 17.6 µm/m-°C
@Temperature 20.0 - 800 °C
Thermal Conductivity 13.7 W/m-K
@Temperature 20.0 - 100 °C
Melting Point 1320 - 1400 °C
Solidus 1320 °C
Liquidus 1400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 20 - 22 %
Copper, Cu <= 0.75 %
Iron, Fe 48 %as balance
Manganese, Mn <= 2.0 %
Molybdenum, Mo 6.0 - 7.0 %
Nickel, Ni 23.5 - 25.5 %
Nitrogen, N 0.18 - 0.25 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 60% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 10% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367)
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work

NL6XN5 / 17960

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.