MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC SABIC® PP 521P PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PP 521P is particularly designed for (biaxially) oriented PP film extrusion with a very specific molecular structure providing the ultimate properties required for the stretching process.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Antiblock Level 0.000 ppm0.000 ppm
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.0 MPa4930 psiISO 527
Tensile Strength, Yield 36.0 MPa5220 psiSpeed of testing: 50 mm/min; ISO 527-2 1A
Elongation at Break 600 %600 %ISO 527
Elongation at Yield 10 %10 %ISO 527-2 1A
Tensile Modulus 1.55 GPa225 ksiSpeed of testing: 1 mm/min; ISO 527-2 1A
Flexural Modulus 1.50 GPa218 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 88.0 °C190 °Fat 50 N (VST/B); Temperature rate: 120°C/h; ISO 306
 155 °C311 °Fat 10 N (VST/A); Temperature rate: 120°C/h; ISO 306/A
 
Descriptive Properties
Anti static agentFalse
Gas fading stabilizedFalseSABIC method
IsotacticityMedium
Molecular Weight DistributionBroad
Nucleating agentFalse

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11193 / 244660

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.