MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® PC 62 One-Component Acrylic Conformal Coating
Categories: Polymer; Thermoset

Material Notes: Loctite Stycast PC 62 provides the following product characteristics:
  • Fluorescent under UV light
  • Provides environmental and mechanical protection
  • Toluene-free alternative
  • Superior toughness and abrasion resistance
  • Easily removable with soldering iron or suitable solvent

Cure: Air dry

Application: Conformal coating

Typical Assembly Applications: Printed circuit board

Loctite Stycast PC 62 conformal coating is a rapid drying acrylic for circuit board protection applications.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.820 g/ccUncured
Solids Content 23 - 26 %
Brookfield Viscosity 52 cPLV, Spindle 1, speed 30 rpm
Thickness 25.0 - 100 micronsFilm Thickness (Adjustable)
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.04e+16 ohm-cm
Insulation Resistance >= 2.30e+14 ohm
@Thickness 0.0500 mm,
Temperature 25.0 °C
50 µm film / 50% RH
Dielectric Constant 2.29
@Frequency 100000 Hz
Dielectric Strength 2000 V/mil
Dissipation Factor 0.12
@Frequency 100000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Drying Temperature 25.0 °C
@Time 86400 sec
Recommended Drying Conditions
 75.0 °C
@Time 2700 sec
Alternative Drying Conditions
Tack-Free Time <= 5.00 min
@Thickness 0.120 mm,
Temperature 25.0 °C
~35% RH (120 µm wet film)
 
Descriptive Properties
AppearanceColorless
Fungus ResistanceNon nutrientPer ASTM G21

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7958 / 255443

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.