MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Ceramics RAHP Reticulated Alumina Hearth Post
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZIRCAR Reticulated Alumina Hearth Posts are rigid highly porous rods and shapes of fine grain dense alumina ceramic. An off-shoot of superalloy casting technology from the aerospace industry, these hearth posts offer low thermal conductivity and excellent strength. They are routinely used as support posts in floors and hearths of many ZIRCAR Furnace Insulation Modules and Insulation Assemblies.

Typical Applications:

  • Support posts in floors and hearths of many ZIRCAR Furnace Insulation Modules and Insulation Assemblies
  • Supports in high temperature process equipment

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³
 
Thermal PropertiesMetricEnglishComments
Softening Point >= 1600 °C>= 2910 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.8 %99.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CZIR906 / 138548

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.