MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Omni Plastics OmniTech™ ASA 407 HSV ASA
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Heat and UV stabilized; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Melt Flow 7.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPaASTM D638
Elongation at Break 10 %ASTM D638
Flexural Strength 69.0 MPaASTM D790
Flexural Modulus 2344 MPaASTM D790
Izod Impact, Notched 214 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Omni Internal Testing
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 480 °F
Middle Barrel Temperature 420 - 500 °F
Front Barrel Temperature 420 - 500 °F
Nozzle Temperature 420 - 500 °F
Melt Temperature 420 - 500 °F
Mold Temperature 80.0 - 140 °F
Drying Temperature 190 °F
Dry Time <= 4.00 hour
Moisture Content <= 0.020 %
Back Pressure 50.0 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 778 Q42 Colored ASA
Omni Plastics OmniTech™ ASA 220 ASA
INEOS Styrolution Luran® S 776S Colored ASA
Lotte Advanced Materials Starex® WR-9100 ASA, Unreinforced
INEOS Styrolution Luran® S 777 K UV Black 56625 ASA

POMNI5139 / 185285

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.