MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ConocoPhillips Hydroclear® Ultra-clean multi-purpose R&O Oil, 100 AGMA Lubricant No. 3
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear Ultra-Clean Multipurpose R&O Oil is specially formulated with proprietary additive chemistry and is recommended for use in a variety of systems which require rust- and oxidation-inhibited oils. The added benefit of mild antiwear protection can significantly increase equipment life, particularly in these hardworking times. These applications include general oiling, air compressors, steam turbines, hydraulic systems, circulating oil systems, oil-filled couplings, centrifugal pumps and lightly loaded gearboxes. Hydroclear Ultra-Clean Multipurpose R&O Oil has been tested and formally approved by Cincinnati Milacron under specifications P-38 (ISO 32), P-55 (46) and P-54 (68). Hydroclear Ultra-Clean Multipurpose R&O Oil exceeds Vickers I-286-S requirements. Hydroclear Ultra-Clean Multipurpose R&O Oil 460 meets the requirements of the Morgoil Lubricant Specification for use in roll-neck bearings. Proven performance in turbines which require antiwear, such as ABB and Alstom (some). Excellent for mist lubrication systems.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.871 g/cc0.0315 lb/in³
Viscosity Measurement 100100Viscosity Index
Saybolt Viscosity at 100°F 516 SUS516 SUS
Saybolt Viscosity at 210°F 65 SUS65 SUS
Kinematic Viscosity at 40°C (104°F) 99 cSt99 cSt
Kinematic Viscosity at 100°C (212°F) 11.2 cSt11.2 cSt
Oxidative Stability 4000 hour4000 hour
ASTM Color 0.500.50
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.400 mm0.0157 in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm762 kV/inNo thickness given.
 
Thermal PropertiesMetricEnglishComments
Pour Point -34.4 °C-30.0 °F
Rotating Bomb Oxidation Test (RBOT) 750 min750 minASTM D 2272
Flash Point 254 °C490 °F
 
Descriptive Properties
ASTM Rust A&BPass
Copper Corrosion1A
Emulsion Characteristics (40-40-0)10 minutes
FZGPass 9 Load StagesASTM D5182
ISO Cleanliness Code14/11Applies to packaged goods only.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON137 / 75174

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.