MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the application requires low shrinkage and excellent adhesion to a wide variety of plastics, metals and circuit board materials. These products give very good environmental protection and dielectric properties over a wide temperature range. The primary difference between the two versions is the LV version has a lower high shear viscosity (higher press flow rate) to provide easier dispensing. The amount of sag upon curing is the same.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccTM R050-16
Water Absorption 0.13 %
@Time 86400 sec
TM R050-35
Viscosity 82000 cP
@Shear Rate 1.00 1/s
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Tensile Strength at Break 5000 psiTM R050-36
Tensile Strength, Ultimate 5000 psiTM R050-36
Tensile Strength, Yield 3000 psiTM R050-36
Elongation at Break 0.00 - 1.0 %TM R050-36
Tensile Modulus 700 ksiTM R050-36
Compressive Yield Strength 12000 psiTM R050-38
Compressive Strength 18000 psiBreak; TM R050-38
 20000 psiUltimate; TM R050-38
Compressive Modulus 550 ksiTM R050-38
Adhesive Bond Strength 1300 psiLap Shear-Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+16 ohm-cm
Dielectric Constant 3.4
@Frequency 100000 Hz
 3.8
@Frequency 100 Hz
Dielectric Strength 440 V/mil
Dissipation Factor 0.030
@Frequency 100 Hz
 0.030
@Frequency 100000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°C
@Temperature <=95.0 °C
Below Tg
 200 µm/m-°C
@Temperature >=95.0 °C
Above Tg
Thermal Conductivity 0.300 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 95.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 10.0 min
@Temperature 150 °C
 15.0 min
@Temperature 120 °C
 30.0 min
@Temperature 110 °C
 
Descriptive Properties
Appearanceblack semi-paste
Mix Ratio by Volumeone part
Side-By-Side Cartridges CapableNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating
Master Bond EP41S-1 Chemically Resistant Two Component Epoxy System
Wacker Semicosil® 964 Conformal Coating
Lord Adhesives CoolTherm™ EP-343 Thermally Conductive Epoxy Conformal Coating

PRESL138 / 101552

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.