MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LEXAN™ Copolymer CXT19UV Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN™ CXT19UV Resin is an UV-stabilized High Heat Polycarbonate Copolymer Resin with Vicat of 190°C and crystal clear transparency. This resin is optimized to have a broad processing window with limited yellowing. It is available in limited transparent colors.

Features: High Heat Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.300 %0.300 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.50 %0.50 %ISO 62-1
Viscosity  15 cP
@Load 2.16 kg,
Temperature 330 °C
15 cP
@Load 4.76 lb,
Temperature 626 °F
MVR cc/10 min; ISO 1133
 30 cP
@Load 2.16 kg,
Temperature 350 °C
30 cP
@Load 4.76 lb,
Temperature 662 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm
@Thickness 3.20 mm
0.0070 - 0.010 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
@Thickness 3.20 mm
0.0070 - 0.010 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  17 g/10 min
@Load 2.16 kg,
Temperature 330 °C
17 g/10 min
@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
 33 g/10 min
@Load 2.16 kg,
Temperature 350 °C
33 g/10 min
@Load 4.76 lb,
Temperature 662 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psi50 mm/min; ASTM D638
 65.0 MPa9430 psi50 mm/min; ISO 527
Tensile Strength, Yield 80.0 MPa11600 psi50 mm/min; ASTM D638
 80.0 MPa11600 psi50 mm/min; ISO 527
Elongation at Break >= 25 %>= 25 %50 mm/min; ASTM D638
 >= 25 %>= 25 %50 mm/min; ISO 527
Elongation at Yield 7.0 %7.0 %50 mm/min; ISO 527
 7.5 %7.5 %50 mm/min; ASTM D638
Tensile Modulus 2.50 GPa363 ksi1 mm/min; ISO 527
 2.60 GPa377 ksi5 mm/min; ASTM D638
Flexural Strength 120 MPa17400 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 120 MPa17400 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.55 GPa370 ksi2 mm/min; ISO 178
 2.60 GPa377 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 80.0 J59.0 ft-lbASTM D256
 70.0 J
@Temperature -30.0 °C
51.6 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*3; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 185 °C365 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 185 °C
@Thickness 3.20 mm
365 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 170 °C338 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 170 °C
@Thickness 3.20 mm
338 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 190 °C374 °FRate B/120; ASTM D1525
 190 °C374 °FRate B/120; ISO 306
Glass Transition Temp, Tg 195 °C383 °Fhalf width; SABIC method
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.6091.609ISO 489
Abbe Number 3030ISO 489
Transmission, Visible  87 %
@Thickness 3.00 mm
87 %
@Thickness 0.118 in
ASTM D1003
 88 %
@Thickness 2.00 mm
88 %
@Thickness 0.0787 in
ASTM D1003
 89 %
@Thickness 1.00 mm
89 %
@Thickness 0.0394 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 305 - 345 °C581 - 653 °F
Zone 2 300 - 340 °C572 - 644 °F
Zone 3 310 - 350 °C590 - 662 °F
Melt Temperature 310 - 350 °C590 - 662 °FInjection Molding
Mold Temperature 120 - 170 °C248 - 338 °F
Drying Temperature 135 °C275 °FInjection Molding
Dry Time 5.00 - 6.00 hour5.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00750 cm0.000984 - 0.00295 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80123 / 288070

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.