MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lord Adhesives PCC40228 Silver Conductor Coating
Categories: Polymer; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: LORD® PCC40228 silver conductive coating is a silver-bearing, one-component latent cure epoxy coating intended for application as a conductive base onto electronic component devices that are barrier plated for surface mount applications.

Features: designed for dip or banding wheel application; may be diluted to suit specific application requirements. cured film forms a highly adherent bond to many substrate compositions. easy to use with good rheological properties.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 8000 cP
@Temperature 25.0 °C
8000 cP
@Temperature 77.0 °F
Brookfield RVT, Spindle 3, 10 rpm
 
Processing PropertiesMetricEnglishComments
Shelf Life  3.00 Month
@Temperature 25.0 °C
3.00 Month
@Temperature 77.0 °F
 6.00 Month
@Temperature 5.00 °C
6.00 Month
@Temperature 41.0 °F
from date of shipment in original, unopened container
 
Descriptive Properties
AppearanceSilver Liquid
Resistivity.0001 maxdried at 100C for 10 min
 .0001 maxcured at 200 C for 30 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9335 / 232691

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.