MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.

  • Recommended for applications requiring excellent flex fatigue resistance.
  • Excellent ozone resistance.
  • Designed for improved UV resistance.

Information provided by Advanced Elastomer Systems

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050.12 in; ASTM D2240
 5757Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 9.260 MPa1343 psi257°F, 70 hr in IRM 903 Oil; ASTM D471
 9.38 MPa1360 psiAir at 302°F, 168 hr; ASTM D573
Tensile Strength, Ultimate 11.7 MPa1700 psiAcross Flow; ASTM D412
Elongation at Break 22.2 %22.2 %Air at 302°F, 168 hr; ASTM D573
 25.2 %25.2 %257°F, 70 hr, in IRM 903 Oil; ASTM D471
 30 %30 %Across Flow; ASTM D412
Tear Strength 86.1 kN/m491 pli73°F, Die C; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 25.2 kV/mm640 kV/inASTM D149
 33.5 kV/mm850 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -36.1 °C-33.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Rear Barrel Temperature 193 °C380 °F
Middle Barrel Temperature 199 °C390 °F
Front Barrel Temperature 204 °C400 °F
Nozzle Temperature 210 - 241 °C410 - 465 °F
Die Temperature 216 °C420 °FExtrusion
Melt Temperature 210 °C410 °FExtrusion
 216 - 232 °C420 - 450 °FProcessing
Mold Temperature 10.0 - 51.7 °C50.0 - 125 °FProcessing
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Moisture Content 0.080 %0.080 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiProcessing
 5.00 - 20.0 MPa725 - 2900 psiExtrusion
Clamp Pressure 41.4 - 68.9 MPa6000 - 10000 psi
Vent Depth 0.00254 cm0.00100 in
Cushion 0.317 - 0.635 cm0.125 - 0.250 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
ColorBlack
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer
RTP Company RTP 2800B-50D HF  Thermoplastic Vulcanizate Elastomer (TPV) 50 Shore D - High Flow
RTP Company RTP 2800B-50A HF  Thermoplastic Vulcanizate Elastomer (TPV) 50 Shore A - High Flow
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer

PADVA076 / 22766

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.