MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® PP G3230AE PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound G3230AE is a 30% short glass fiber reinforced Polypropylene for under-the-hood and structural applications. The base material is a PP homopolymer, optimized for low emission values. The glass fibres are chemically coupled to the PP matrix. This material has been designed to combine a good performance profile with fast processing. SABIC® PPcompound G3230AE is a designated automotive grade. IMDS ID: 325273910

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³Injection molded sample ISO527-1A; ISO 1183
Filler Content 30 %30 %SABIC method
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inInjection molded plaque 65x65x3.2mm; SABIC method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 97.0 MPa14100 psiISO 527/1A
Elongation at Break 3.7 %3.7 %ISO 527/1A
Tensile Modulus 6.50 GPa943 ksiISO 527/1A
Flexural Modulus 6.30 GPa914 ksiISO 178/1A
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²N.B.: No Break; ISO 180/1A
Charpy Impact Unnotched 5.30 J/cm²25.2 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear  31.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
17.2 µin/in-°F
@Temperature 73.4 - 176 °F
ASTM D696
 32.0 µm/m-°C
@Temperature -30.0 - 100 °C
17.8 µin/in-°F
@Temperature -22.0 - 212 °F
ISO 11359-2
 33.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
18.3 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11532 / 244999

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.