MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ganpati Exim SP-W
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C22 H22 O

Properties : SP-C, SP-W are grayish-white powder which is adsorbed on mineral stuffing by SP and they are dissolved in ethanol, acetone, benzene, aether and other organic and other organic dissolvent, insoluble in water

Application : The article is a non-polluted anti-ageing agent. It has a good protective effect for heat proof ageing, light-resistant, etc. And used in natural rubber , and other light –color rubber products with the features of undiscolor, no pollution and nonspray frost and easy dispersing. The quantity of used for SP is 0.5-3.0 portion. It can be used as rubber latex after emulsification. The cost is lower. The function of SP-C, SP-W is the same as SP. SP-C, SP-W are antioxidant of polyfomaldehgde and polyolefine in plastic industry. The quantity of use is 0.01-0.5 portion.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.075 - 1.088 g/cc0.03884 - 0.03931 lb/in³
Viscosity 3200 - 5000 cP3200 - 5000 cP
Molecular Weight 322 g/mol322 g/mol
Ash 0.050 %0.050 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.599 - 1.60151.599 - 1.6015
 
Descriptive Properties
Appearancelight yellow transparent stickiness liquid
Heating Loss0.01

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI081 / 317365

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.