MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Claytone® IMG 400 Gellant for Oil Mud Systems
Categories: Fluid; Lubricant; Clay Gellant

Material Notes: Claytone IMG-400 is high yield organophilic clay gellant for use in oil mud systems. Mud systems formulated with Claytone IMG-400 to desired viscosity and yield point require up to 50% less gellant than with typical low yield organophilic clays. Actual savings will depend upon the specific formulation and desired rheological properties. Claytone IMG-400 is manufactured under a strict quality control program which assures the user of consistent performance in all oil mud systems.

Applications:

  • Oil mud systems

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 42.0 lb/ft³
Particle Mesh Size 200 Mesh<15%
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 2.0 %
@Temperature 105.2 °C
loss
 
Descriptive Properties
Yield400 bbls/ton15 cps Diesel Oil/Water-95/5 )

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Claytone® HT Rheological Additive
BYK Claytone® ER Organophilic Bentonite
BYK Claytone® EM Gellant for Oil Mud Systems
BYK Claytone® APA Rheological Additive
BYK Claytone® AF Rheological Additive

PBYK026 / 185023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.