MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM  (discontinued **)
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.

Data provided by the manufacturer, Solvay Advanced Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccASTM D792
Water Absorption 0.19 %24 hrs; ASTM D570
Moisture Absorption at Equilibrium 1.78 %at 65% RH per Solvay test
Linear Mold Shrinkage, Flow 0.0025 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 185 MPaASTM D638
Elongation at Break 2.3 %ASTM D638
Tensile Modulus 13.0 GPaASTM D638
Flexural Yield Strength 275 MPaASTM D790
Flexural Modulus 11.0 GPaASTM D790
Izod Impact, Notched 0.600 J/cmASTM D256
Izod Impact, Unnotched 4.50 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.00e+15 ohm-cmASTM D257
Dielectric Constant 3.8
@Frequency 110 Hz
ASTM D150
Dielectric Strength 31.0 kV/mmASTM D149
Dissipation Factor 0.010
@Frequency 110 Hz
ASTM D150
Arc Resistance >= 60 secASTM D495
Comparative Tracking Index >= 250 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.300 W/m-KASTM C177
Melting Point 240 °C
Deflection Temperature at 1.8 MPa (264 psi) 230 °CHDT/A; ASTM D648
UL RTI, Electrical 120 °C
@Thickness 1.50 - 3.00 mm
UL RTI, Mechanical with Impact 105 °C
@Thickness 1.50 - 3.00 mm
UL RTI, Mechanical without Impact 105 °C
@Thickness 1.50 mm
 120 °C
@Thickness 3.00 mm
Flammability, UL94 V-0
@Thickness 1.60 mm
UL Rating; Solvay test
Oxygen Index 31.5 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Feed Temperature 250 - 280 °C
Rear Barrel Temperature 250 - 280 °CCompression Zone
Middle Barrel Temperature 250 - 280 °CHomogenization Zone
Front Barrel Temperature 260 - 290 °CNozzle Zone
Melt Temperature <= 270 °C
Mold Temperature 120 - 140 °CNeeded to develop high crystallinity
Injection Pressure 50.0 - 250 MPa
Hold Pressure 30.0 - 150 MPa
Back Pressure 0.000 - 1.00 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 299 K X 138347 B Polyarylamide (PAA); Glass Fiber - Flame Retardant - Preliminary Datasheet
Envalior Stanyl® TE250F6 PA46-GF30 FR(17), Dry, 30% Glass Filled, Heat Stabilized, Flame Retardant
Overview of materials for Polyarylamide, Glass Fiber Filled
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
RTP Company RTP 205 K Polyarylamide (PAA), Glass Fiber

PSOLN6 / 68326

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.