MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polynt ARMORCOTE® 966 Series Metallic Gel Coat
Categories: Polymer; Thermoset

Material Notes: ARMORCOTE® 966 Series metallic gel coats are used in passenger, camper, utility, and recreation vehicles, decorative structural components, and for marine vehicle surfaces above the water line (not recommended for water immersion service). ARMORCOTE® 966 Series is Polynt Composites’ best system for weathering resistance in a metallic gel coat ARMORCOTE® 966 Series meets the EPA National Emission Standards for Hazardous Air Pollutants (NESHAP) for both Marine Manufacturing and Reinforced Composites Production.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 14500 cP14500 cPRVF #4 Spindle @ 4 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 26.1 °C79.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 67.5 min1.13 hourLay-up Time
Gel Time 15.5 min15.5 minArkema Luperox® @ 1.8% DDM-9
 
Descriptive Properties
Sag ResistanceGood @ 24 mils wet
Thixotropic Index5.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9181 / 231776

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.