MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Inno-Comp INNOPOL® CS 3-3130 B 25% Talc-Filled Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: INNOPOL® CS 3-3130 B is a black colored, 25% talc-filled polypropylene compound.

INNOPOL® CS 3-3130 B is a recommended for producing injection molded products where the required property is high strength and high stiffness.

All information provided by INNO-COMP.

Key Words: PP-B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc
@Temperature 23.0 °C
0.0394 lb/in³
@Temperature 73.4 °F
ISO 1183
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.0 MPa4350 psi50 mm/min; ISO 527-1,-2
Elongation at Yield 3.0 %3.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 3.00 GPa435 ksi1 mm/min; ISO 527-1,-2
Flexural Modulus 3.20 GPa464 ksi2 mm/min; ISO 178
Charpy Impact, Notched  0.170 J/cm²
@Temperature -20.0 °C
0.809 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 0.350 J/cm²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FISO 75-1,-2
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 10% Talc Filler
Overview of materials for Polypropylene with 30% Talc Filler
A. Schulman TPP30AJ41BK 30% Talc Filled, Heat-Stabilized, Homopolymer Polypropylene containing 25% P.C.R.
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled
Arkema Appryl® CZU 0525 Polypropylene, 25% Talc Filled

PINNO063 / 82724

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.