MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SunChemical Gwent C2040902D6 Carbon Ink for Electro Luminescent Lamps  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: This product is based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has excellent adhesion, chemical and environmental resistance properties. Although originally designed as a Back Electrode, the excellent conductivity of this ink makes it suitable as a replacement for Silver Ink in smaller EL Lamps.

This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use to ensure complete homogeneity.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 6000 - 10000 cP
@Shear Rate 50 1/s,
Temperature 25.0 °C
6000 - 10000 cP
@Shear Rate 50 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer with the PK1.1°
Thickness 14.0 - 16.0 microns0.551 - 0.630 milCured film
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 60 ohm<= 60 ohmat 25 microns thick
 
Processing PropertiesMetricEnglishComments
Cure Time  3.00 min
@Temperature 130 °C
0.0500 hour
@Temperature 266 °F
belt dryer
 10.0 min
@Temperature 130 °C
0.167 hour
@Temperature 266 °F
box oven
Shelf Life 3.00 Month3.00 Monthat 20°C maximum
 6.00 Month6.00 Monthat 5°C maximum
 
Descriptive Properties
Printing Mesh counts/inch180 to 230stainless steel screens

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WGEM017 / 75870

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.