MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical Raw C5
Categories: Fluid

Material Notes: Structure & Characteristics: Synthesized by vacuum-distillation of pyrolysis gasoline produced from naphtha pyrolysis process. The content of isoprene as C5 without undergoing hydration process is higher than 12%. Although it is in liquid form in room temperature and pressure, it easily vaporizes in room temperature.

Uses: Isoprene is extracted to produce isoprene rubber.

CAS: 78-78-4 and 109-66-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.668 - 0.672 g/cc0.668 - 0.672 g/ccASTM D287
Volatiles 100 %100 %
Vapor Pressure 1.16 bar
@Temperature 40.0 °C
872 torr
@Temperature 104 °F
Vapor Density=2.5
 
Thermal PropertiesMetricEnglishComments
Melting Point -130 °C-202 °F
Boiling Point 40.6 °C105 °F
Flash Point <= -57.0 °C<= -70.6 °F
 
Descriptive Properties
Components1,3-Pentadiene9.5%
 2-methy-2-pentene0.65%
 2-Pentene5.8%
 Benzene0.75%
 C4 LIGHTERS0.65%
 C6 & HEAVIERS(EXCLUDINGDCPD)3.2%
 CARBONYLS(AS CH3CHO500-1000 ppm, ZEON M-023A
 cyclo-Pentadiene17.6%
 cyclo-Pentene7.46%
 iso-Pentane15.48%
 Isoprene13.43%
 ISOPRENE13-14%
 n-Hexane8.5%
 n-Pentane20.83%
 T-S(as CS2)2 ppm, ASTM D5453

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLAY764 / 148774

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.