MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Solvay Vac-Pak® HS800 Vacuum bagging film
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Vacuum bagging film. Ideally suited to high temperature and pressure applications.

Features & Benefits:

  • Heat stabilized co-extruded film produced from modified nylon resin
  • Ideal for advanced composite fabrication and adhesive bonding as well as other high temperature/pressure applications where softness and workability are essential
  • The co-extrusion process combines multiple layers of resin flow into film prior to exiting the extrusion die. This process represents the most advanced state of the art technology in blow film production
  • Can be heat seamed to meet any custom shape requirements

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 50.0 microns
 75.0 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 12000 psiASTM D882
Elongation at Break 300 %ASTM D882
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 191 °C
 
Descriptive Properties
ColorGold tinted
Yield11.6 m2/kg75 µm
 17.3 m2/kg50 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Gold Alloy
Gold, Au; 18K, White Composition Spec (UNS P00275)
Gold, Au; 10K, Red (UNS P00145)
Gold, Au
Gold 99.99%, Be Modified

PCYTED302 / 180604

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.