MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Master Bond Mastersil 702 One Component, Room Temperature Curing Silicone Elastomer
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Master Bond Master Sil 702 is ready-to-use, one component high performance silicone elastomer compound for bonding and sealing. Master Sil 702 is heat resistant to 450°F. It is supplied as an easy to apply paste and reacts with moisture in the air to form a durable silicone rubber. Master Sil 702 compound will adhere to many substrates including glass, ceramics, metals, silicone rubber and most plastics.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3333
Tensile Strength, Yield 5.17 MPa750 psi
Elongation at Yield 620 %620 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -59.4 °C-75.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 - 2880 min
@Temperature 23.0 °C
24.0 - 48.0 hour
@Temperature 73.4 °F
 
Descriptive Properties
ColorTranslucent, gray or black
Set-Up Time, minutes15-20At Room Temperature
ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Humiseal 1C49 Silicone Conformal Coating
Henkel Loctite® Shadowcure™ 5293 Silicone Coating
Henkel Loctite® Output™ 5404 Heat Cure Silicone
Henkel Loctite® Nuva-Sil® 5092 Non-corrosive Potting
Henkel Loctite® Nuva-Sil® 5088 Potting Compound

PMASTB168 / 52325

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.