Plasticized, heat- and light- stabilized polyamide 12 compound. VESTAMID LX9002 black 9.7507 is a plasticized polyamide 12 compound with heat and light stabilizer for the extrusion of multilayer tubing 2030 and 2040 developed by Evonik Degussa GmbH. VESTAMID LX9002 is characterized by easy processing as well as by a high impact strength at low temperatures. VESTAMID LX9002 is recommended in order to attain an excellent bonding with DYFLOR X7394. VESTAMID LX9002 is supplied as cylindrical pellets, ready for use, in moisture-proof bags. It has to be noticed that material data measured on test specimens, do not provide sufficient information to draw conclusions on the final performance of the resin when used in a multilayer tubing. Property data for dry samples. Information provided by Evonik. |