MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Crosspolimeri FRAGOM G/478 NAT Flame Retardant Halogen Free Polyolefine
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant halogen free polyolefine compounds.

FRAGOM G/478 NAT: flame retardant crosslinkable compound having good temperature index and oxygen index, suitable for cable sheathing and insulation. It is a conveniently grafted compound able to react in presence of moisture and of a catalyst. We suggest our catalyst type MAC/308 PSL or MAC/408 PSL (more reactive type) to extrude with low compression screw. To use in solar cables sheathing ( TUV ) we suggest to add 7/8 % of catalyst MAC/308 SPUV. REACTION BETWEEN GRAFTING AND CATALYST These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 95/5

Certify: BS7211 EI5,VDE0207 HJ1,AZ/NZS R-HF-110,CEI 2011 G10-M2

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
Melt Flow  6.0 - 8.0 g/10 min
@Load 21.6 kg,
Temperature 150 °C
6.0 - 8.0 g/10 min
@Load 47.6 lb,
Temperature 302 °F
Internal System
 10 - 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10 - 20 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3838ASTM D2240
Tensile Strength >= 11.0 MPa>= 1600 psiIEC 60811
 >= 9.68 MPa
@Temperature 135 °C,
Time 605000 sec
>= 1400 psi
@Temperature 275 °F,
Time 168 hour
Heat Ageing; IEC 60811
 >= 15.4 MPa
@Temperature 100 °C,
Time 14400 sec
>= 2230 psi
@Temperature 212 °F,
Time 4.00 hour
Ageing in IRM 902 oil; IEC 60811
Elongation at Break >= 200 %>= 200 %IEC 60811
 >= 50 %
@Temperature 190 °C
>= 50 %
@Temperature 374 °F
Heat Ageing; TUV* / M21*
 >= 212 %
@Temperature 135 °C,
Time 605000 sec
>= 212 %
@Temperature 275 °F,
Time 168 hour
Heat Ageing; IEC 60811
 >= 280 %
@Temperature 100 °C,
Time 14400 sec
>= 280 %
@Temperature 212 °F,
Time 4.00 hour
Ageing in IRM 902 oil; IEC 60811
100% Modulus 100 MPa14500 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmIEC 167
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 34 %34 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 80.0 - 90.0 °C176 - 194 °F
Zone 2 100 - 115 °C212 - 239 °F
Zone 3 145 °C293 °F
Zone 4 160 °C320 °F
Die Temperature 175 °C347 °F
Head Temperature 170 °C338 °F
 
Descriptive Properties
Corrosivity of gases evolved>4,4 pHIEC 60754-2
Halogen Content< 0,3%IEC 60754-1
Hot Set Test+5%Residual Value, IEC 60811
 0.5250°C - 20 N/cm2, IEC 60811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS064 / 294148

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.