MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Titanium Grade 18 Ti-3Al-2.5V-0.05Pd
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: ASTM B265 Grade

Mechanical property data for annealed samples

UNS R56322

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 15
Tensile Strength, Ultimate 621 - 740 MPa
Tensile Strength, Yield 483 - 607 MPa
@Strain 0.2 %
Elongation at Break 15 - 17 %
Modulus of Elasticity 91.0 - 107 GPa
Charpy Impact 48.0 JV Notch
Bend Radius, Minimum >= 2.5 t2 mm sheet
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 2.5 - 3.5 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.25 %
Nitrogen, N <= 0.030 %
Other, each <= 0.050 %
Other, total <= 0.30 %
Oxygen, O <= 0.15 %
Palladium, Pd 0.040 - 0.080 %
Titanium, Ti 92.595 - 95.16 %As Balance
Vanadium, V 2.3 - 3.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 19 Ti-3Al-8V-6Cr-4Mo-4Zr
Titanium Grade 24 Ti-6Al-4V-0.06Pd
Titanium Grade 25 Ti-6Al-4V-0.5Ni-0.06Pd
Titanium Grade 20 Ti-8V-6Cr-4Zr-4Mo-3Al-0.06Pd
Titanium Grade 27 Ti-0.1Ru

MTQ905 / 100326

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.