MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Aged 490°C
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Alloy was solution treated before aging. Good ductility and fabrication properties, aging yields extremely high strengths, low density.

Applications: Areospace and missile applications, springs

5 other heat treatments of this alloy are in MatWeb.

Key Words: Ti-13-11-3; UNS R58010; B120VCA
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.82 g/cc0.174 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 485485Estimated from Rockwell C.
Hardness, Knoop 535535Estimated from Rockwell C.
Hardness, Rockwell C 5050
Hardness, Vickers 511511Estimated from Rockwell C.
Tensile Strength, Ultimate 1460 MPa212000 psi
Tensile Strength, Yield 1300 MPa189000 psi
Elongation at Break 23 %23 %
Reduction of Area 6.0 %6.0 %
Tensile Modulus 110 GPa16000 ksi
Poissons Ratio 0.300.30annealed
Shear Modulus 43.0 GPa6240 ksiAnnealed Sample
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000140 ohm-cm0.000140 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.67 µm/m-°C
@Temperature 20.0 - 95.0 °C
5.37 µin/in-°F
@Temperature 68.0 - 203 °F
 9.99 µm/m-°C
@Temperature 20.0 - 315 °C
5.55 µin/in-°F
@Temperature 68.0 - 599 °F
average
 10.44 µm/m-°C
@Temperature 20.0 - 650 °C
5.800 µin/in-°F
@Temperature 68.0 - 1200 °F
average
Specific Heat Capacity  0.545 J/g-°C
@Temperature 20.0 °C
0.130 BTU/lb-°F
@Temperature 68.0 °F
 0.833 J/g-°C
@Temperature 425 °C
0.199 BTU/lb-°F
@Temperature 797 °F
Thermal Conductivity  6.90 W/m-K
@Temperature 20.0 °C
47.9 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 17.1 W/m-K
@Temperature 425 °C
119 BTU-in/hr-ft²-°F
@Temperature 797 °F
Beta Transus 700 °C1290 °FCommercial grade; lower for grades with lower oxygen content
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.0 %3.0 %
Carbon, C <= 0.10 %<= 0.10 %
Chromium, Cr 11 %11 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.35 %<= 0.35 %
Nitrogen, N <= 0.080 %<= 0.080 %
Oxygen, O <= 0.20 %<= 0.20 %
Titanium, Ti 73 %73 %
Vanadium, V 13 %13 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) SolnTreat; Age 450°C
Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 850°C (1560°F) + Aged 510°C 8 hr
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Aged 400°C
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Solution Treated
Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 800°C, 30 min.

MTB313 / 14185

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.