MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Label-Lyte™ ROSO 50LR210 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A clear, machine-direction shrinkable, one-side treated, polypropylene film. This film is designed for use as a monoweb in roll-fed labeling of contoured containers, such as aluminum and steel beverage cans, beaded metal cans, aerosol containers, and contoured glass and plastic bottles. The treated clear layer is for printing and hot melt adhesion to the container and is intended to be reverse-printed with water-based or solvent-based flexo and gravure inks and UV-cured inks. The machinable high gloss layer is designed for robust machinability on all roll-fed labelers.

Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, North America and South America

Key Features:

  • Outstanding, consistent, and uniform machine-direction shrinkage, up to 19%
  • Excellent clarity and gloss
  • Excellent ink and hot melt adhesion
  • Consistent machinability on all roll-fed label machines
Applications:
  • Beverage, Carbonated
  • Beverage, Mineral Waters
  • Dairy Products
  • Dry Foods and Beverage Powders
Uses:
  • Reel-Fed Shrink Labels
Processing Method: Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, UV Flexographic Printing and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milExxonMobil Method
Coating Weight 44.8 g/m²28.0 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.350.35Untreated Surface; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 19 %
@Temperature 135 °C
19 %
@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 2.0 %
@Temperature 135 °C
2.0 %
@Temperature 275 °F
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 2.8 %2.8 %ExxonMobil Method
Gloss 82 %82 %45°; ExxonMobil Method
 
Descriptive Properties
Treatment40 dyne/cmPrint Surface
Yield15500 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Niagara LaSalle Fatigue-Proof® Cold Finished Steel Bar
ExxonMobil Mobilgrease HTR
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel
ATI Allegheny Ludlum K12® Dual Hardness Steel
Assab Steels HOTVAR Hot Work Steel

PEX99562 / 175798

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.